  1. Thermite II... or A better way to make Thermite        by Jolly Roger
  2.  
  3. Thermite is nasty shit. Here is a good and easy way to make it. 
  4. The first step is to get some iron-oxide (which is RUST!). Here is 
  5. a good way to make large quantities in a short time:
  6.  
  7. - Get a DC convertor like the one used on a train set. Cut the 
  8. connector off, seperate the wires, and strip them both.
  9.  
  10. - Now you need a jar of water with a tablespoon or so of sodium 
  11. chloride (which is SALT!) added to it. This makes the water 
  12. conductive.
  13.  
  14. - Now insert both wires into the mixture (I am assuming you 
  15. plugged the convertor in...) and let them sit for five minutes. 
  16. One of them will start bubbling more than the other. This is the 
  17. POSITIVE(+) wire. If you do not do this test right, the final 
  18. product will be the opposite (chemically) of rust, which is RUST 
  19. ACID. You have no use for this here (although it IS useful!).
  20.  
  21. - Anyway, put the nail tied to the positive wire into the jar. Now 
  22. put the negative wire in the other end. Now let it sit overnight 
  23. and in the morning scrape the rust off of the nail & repeat until 
  24. you got a bunch of rust on the bottom of the glass. Be generous 
  25. with your rust collection. If you are going through the trouble of 
  26. making thermite, you might as well make a lot, right?
  27.  
  28. - Now remove the excess water and pour the crusty solution onto a 
  29. cookie sheet. Dry it in the sun for a few hours, or inside 
  30. overnight. It should be an orange-brown color (although I have 
  31. seen it in many different colors! Sometimes the color gets fucked 
  32. up, what can I say... but it is still iron oxide!)
  33.  
  34. - Crush the rust into a fine powder and heat it in a cast-iron pot 
  35. until it is red. Now mix the pure iron oxide with pure alluminum 
  36. filinos which can be bought or filed down by hand from an aluminum 
  37. tube or bar. The ratio or iron oxide to aluminum is 8 grams to 3 
  38. grams.
  39.  
  40. - Congrats! You have just made THERMITE! Now, to light it...
  41.  
  42. - Thermite requires a LOT of heat (more than a blow torch!) to 
  43. ignite. However, a magnesium ribbon (which is sorta hard to find.. 
  44. call around) will do the trick.  It takes the heat from the 
  45. burning magnesium to light the thermite.
  46.  
  47. - Now when you see your victim's car, pour a fifty-cent sized pile 
  48. onto his hood, stick the ribbon in it, and light the ribbon with 
  49. the blow torch. Now chuckle as you watch it burn through the hood, 
  50. the block, the axle, and the pavement. BE CAREFUL! The ideal 
  51. mixtures can vaporize CARBON STEEL! Another idea is to use 
  52. thermite to get into pay phone cash boxes. HAVE FUN!! -Jolly Roger-
  53.  
  54.  